L'image affichée est à des fins de représentation uniquement et peut ne pas refléter le produit réel.
Diameters / Packaging
|
Diameters |
5 kg Tube |
|---|---|
| 2.4 mm | T5CRMO-24 |
Détails
Low Alloy Steel • AWS A5.28M ER80S-B6
Traits
- B6 alloyed steel: 5% chromium, 0.5% molybdenum alloyed steel consumable for elevated temperature service up to 600°C (1112°F)
- Designed for high strength and improved corrosion resistance with hot hydrogen gas, super-heated steam, and Sulphur crude oil
Applications typiques
- Pressure Vessels
- Piping
- Heat Exchangers
Gaz de protection
- 100% Argon
Disclaimers
Des informations de service
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
| CONFORMANCES | SPECIFICATION | CLASSIFICATION |
|---|---|---|
| AWS | AWS A5.28 | ER80S-B6 |
MECHANICAL PROPERTIES
| Classification | Postweld Heat Treatment | Shielding Gas | Polarity |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
|---|---|---|---|---|---|---|
| ER80S-B6 Requirement | 100% Ar | DC- | 470 (68) min. | 550 (80) min. | 17 min. | |
| Typical Result, Stress relieved | 1 hour @ 750°C (1380°F) | 100% Ar | DC- | 560 (82) | 670 (97) | 25 |
DEPOSIT COMPOSITION
| Classification | Shielding Gas |
|---|---|
| Typical Result | 100% Ar |
WIRE COMPOSITION
| Classification | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %Total Cu |
|---|---|---|---|---|---|---|---|---|---|
| ER80S-B6 Requirement | 0.10 min. | 4.50 - 6.00 | 0.40 - 0.70 | 0.45 - 0.65 | 0.60 max. | 0.025 max. | 0.025 max. | 0.50 min. | 0.35 max. |
| Typical Result | 0.08 | 5.66 | 0.48 | 0.56 | 0.10 | 0.010 | 0.008 | 0.40 | 0.10 |