L'image affichée est à des fins de représentation uniquement et peut ne pas refléter le produit réel.
Diameters / Packaging
|
Diameters |
55 lb (25 kg) Steel Spool |
|---|---|
| 1/8 in (3.2 mm) | SA617125726 |
Détails
TECHALLOY® 617 ideal for use when optimum strength and oxidation resistance are required at temperatures from 1500°F (815°C) up to 2100°F (1150°C).
Traits
- The weld metal provides optimum strength and oxidation resistance from 1500°F (815°C) up to 2100°F (1150°C)
- Q2 Lot® - Certificate showing actual wire composition available online
Applications typiques
- Used for MIG, TIG and SAW welding of nickel-chrome-cobalt-molybdenum alloys
- Process Industries
- Petrochemical
Positions de soudage
- All
Gaz de protection
- SAW P2000
Disclaimers
Des informations de service
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
| CONFORMANCES | SPECIFICATION | CLASSIFICATION |
|---|---|---|
| AWS | AWS A5.14 | ERNiCrCoMo-1 |
| CWB | CWB AWS A5.14 | ERNiCrCoMo-1 |
WIRE COMPOSITION
| Classification | %Al | %C | %Co | %Cr | %Cu | %Fe | %Mn | %Mo | %Ni | %P | %S | %Si | %Ti |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ERNiCrCoMo-1 Requirement | 0.8 - 1.5 | 0.05 - 0.15 | 10.0 - 15.0 | 20.0 - 24.0 | 0.50 max. | 3.0 max. | 1.0 max. | 8.0 - 10.0 | Remainder | 0.03 max. | 0.015 max. | 1.0 max. | 0.60 max. |
| Typical Result | 1.4 | 0.07 | 11.6 | 22.9 | 0.02 | 0.5 | 0.3 | 8.8 | 54 | 0.003 max. | 0.003 max. | 0.0 max. | 0.36 |
TYPICAL OPERATING PROCEDURES
| Diameter | Polarity |
Voltage
volts |
Approx. Current
amps |
Flux |
|---|---|---|---|---|