L'image affichée est à des fins de représentation uniquement et peut ne pas refléter le produit réel.
Diameters / Packaging
|
Diameters |
33 lb (15 kg) Steel Spool |
|---|---|
| 0.035 in (0.9 mm) | MG718035667 |
| 0.045 in (1.1 mm) | MG718045667 |
| 1/16 in (1.6 mm) | MG718062667 |
Détails
TECHALLOY® 718 ideal for welding high strength aircraft components and liquid rocket components involving cryogenic temperatures, as it can be age hardened to higher strengths operation.
Traits
- This alloy can be age hardened to higher strengths
- Q2 Lot® - Certificate showing actual wire composition available online
Applications typiques
- Used for welding alloys 718, 706 and X-750
- Mainly used for welding high strength aircraft components and liquid rocket components involving cryogenic temperatures
- General Fabrication
Positions de soudage
- All
Gaz de protection
- MIG 75% Argon / 25% Helium
Disclaimers
Des informations de service
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
| CONFORMANCES | SPECIFICATION | CLASSIFICATION |
|---|---|---|
| AWS | AWS A5.14 | ERNiFeCr-2 |
| CWB | AWS A5.14 | ERNiFeCr-2 |
WIRE COMPOSITION
| Classification | %Al | %B | %C | %Cr | %Cu | %Fe | %Mn | %Mo | %P | %S | %Si | %Ti | %Nb+Ta | %Ni+Co |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ERNiFeCr-2 Requirement | 0.20 - 0.80 | 0.006 max. | 0.08 max. | 17.0 - 21.0 | 0.30 max. | Remainder | 0.35 max. | 2.80 - 3.30 | 0.015 max. | 0.015 max. | 0.35 max. | 0.65 - 1.15 | 4.75 - 5.50 | 50.0 - 55.0 |
| Typical Result | 0.50 | 0.005 | 0.06 | 17.5 | 0.02 | 20.2 | 0.06 | 3.04 | 0.003 max. | 0.003 max. | 0.04 | 0.93 | 5.11 | 52.5 |
TYPICAL OPERATING PROCEDURES
| Diameter | Shielding Gas | Polarity |
Voltage
volts |
Approx. Current
amps |
|---|---|---|---|---|
| .035" (0.9 mm) | 75% Ar, 25% He | DC+ | 26-29 | 150-190 |
| .045" (1.1 mm) | 75% Ar, 25% He | DC+ | 28-32 | 180-220 |
| 1/16" (1.6 mm) | 75% Ar, 25% He | DC+ | 29-33 | 200-250 |