Dry packaging LINCOLN stick electrode (VPMD)
The image shown is for representation purposes only and may not reflect the actual product.

Diameters / Packaging

Diameters
VPMD 10,8 KG (6 x 1,8 KG, approx. 540 pcs)
VPMD 12 KG (6 x 2 KG, approx. 318 pcs)
VPMD 15,6 KG (6 x 2,6 KG, approx. 222 pcs)
2.5x350 mm CHROMET2-25-2
3.2x350 mm CHROMET2-32-2
4.0x450 mm CHROMET2-40-2

Chromet® 2 (SL 20G)

Stick (SMAW) | CHROMET2-40-2

CLASSIFICATIONS:
AWS A5.5 : E9018-B3 H4R
EN ISO 3580-A : E CrMo2 B 3 2 H5
EN ISO 3580-B : E 6216-2C1M

Stick electrode Chromet® 2 (SL 20G) - 4.0x450 mm - VPMD 16.2 KG (approx. 222 pcs)

DETAILS

Basic very low hydrogen all position electrode (HDM< 5 ml/100g)

Features

  • For welding creep and hydrogen resistant CrMo-steels
  • Maximum service temperature 600°C
  • DC-welding preferred
  • 115 - 120% recovery

Service Information

Documentation

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.5 E9018-B3 H4R
ISO ISO 3580-A E CrMo2 B 3 2 H5
TUV ISO 3580-A E CrMo2 B 3 2

MECHANICAL PROPERTIES

Classification Postweld Heat Treatment Yield Strength @ 0.2% Offset
MPa (ksi)
Tensile Strength
MPa (ksi)
Elongation
%
E9018-B3 H4R Requirement 530 (77) min. 620 (90) min. 17 min.
E CrMo2 B 3 2 H5 Requirement 400 (58) min. 500 (72) min. 18 min.
Typical Result, Stress relieved 690°C/1h 570 (83) 670 (97) 20

DEPOSIT COMPOSITION

Classification %C %Cr %Cu %Mn %Mo %Nb %Ni %P %S %Si
E9018-B3 H4R Requirement 0.05 - 0.12 2.00 - 2.50 0.90 max. 0.90 - 1.20 0.03 max. 0.03 max. 0.80 max.
E CrMo2 B 3 2 H5 Requirement 0.05 - 0.12 2.0 - 2.6 0.3 max. 0.40 - 1.30 0.90 - 1.30 0.01 max. 0.3 max. 0.030 max. 0.025 max. 0.80 max.
Typical Result 0.07 2.30 0.1 0.80 1.00 0.01 0.1 0.020 0.010 0.60