Question Mark

Question Mark | Tuesday, December 22, 2020 | United States



Expert answers help welders understand common shop challenges, improve TIG welding skills, troubleshoot equipment issues, and gain confidence when working with sheet metal and larger weldments.

Question Mark Department Header

image
image
image

Why does my tungsten look black and burnt after welding?

TIG welding with a contaminated tungsten can be a frustrating experience. When learning how to TIG weld, you’ll need to maintain a clear path in your work space to the grinder to keep that electrode sharp and clean. As you develop skill, the trips to the grinder will be less frequent. When you weld after dressing the electrode and it turns black and burnt immediately after, it’s because you don’t have sufficient post flow to allow the tungsten to cool in a protected atmosphere. Some welding machines establish the post flow automatically, according to the diameter of the tungsten you’re using. The more sophisticated machines have a control to adjust the amount of post flow. It’s also possible that you have a loose connection, a hole in the line or even an incorrectly assembled torch. Whichever the case, the black and burnt coloration suggests that the tungsten is not getting enough gas flow after the arc is extinguished.

image

How big can I make a single-pass weld?

Making larger welds on thicker materials is a process of combining several smaller welds fused together to fill the weld joint. No matter the process, the puddle can only fuse and penetrate into the base metal so far, unless you’re using a very powerful machine. The knowledge and skill required to perform multi-pass welds will change depending on position and process. Different welding positions require different techniques to ensure proper fusion when creating a multi-pass weld. So the ultimate answer to the question is: the code book determines how big your single-pass weld can be while still maintaining weld integrity with different welding processes. Again, when you begin welding materials thicker than 3/16 inch thick, the situation changes. Joint preparation changes, welding technique changes and the number of welds required to produce the weld changes.

What is the most important component of learning to TIG weld?

A good question, with a much simpler answer than you might think. Learning to be a competent TIG welder requires two components. The first is learning a little about the process of welding — what polarity to use, what cover gas to use, filler metal type and size, and voltage/amperage relationships. These elements make up the science of how a weld works, and you need to understand them in order to understand what happens during the welding process.

The second component is learning the technique of welding. This requires developing eye-hand coordination and muscle memory – your eyes’ ability to see the weld, your brain’s ability to process what it sees, and your hands’ ability to react to the puddle.

Some of the most important factors a beginning welder should focus on are comfort, the position of head and hands to maximize visual access to the puddle, and an understanding of how the puddle reacts to things like arc length, torch angle and change in travel speed.

Simply put, it takes time and practice to develop the necessary skills to become a competent welder.

image
image

I have heard several people refer to “hammer welding” sheet metal, what does that mean?

I’m not entirely certain where the term originated. It certainly isn’t used in any code books, but it’s a recognized technique – and if you work with thin sheet metal, it’s an important technique to learn.

When we weld sheet metal on a car, for example, the material is going to distort. There’s no stopping it. So you have one of two choices to fix the distorted panel on that car. You can wipe big globs of a polyester surface enhancer into the distorted space, or you can hammer weld. Hammer welding is the process of hammering the weld against a dolly to stretch the weld back into place. Welding creates shrinkage, and in order to reverse the shrinkage we have to stretch the material back into place. Hammering the weld on a dolly will return the metal to its original condition. TIG welds are soft enough to hammer, but MIG welds can crack from hammering. This is why, when welders operate sheet metal that will be finished, they usually use the TIG process.

image