Detalles
EXCALIBUR® 385-16 requires minimal heat input welding procedures be used to avoid solidification cracking. Often used in fabrication of equipment and vessels for handling and storage of sulfuric acid and phosphoric acid.
Características
- The weld metal is fully austenitic
- Minimal heat input welding procedures should be used to avoid solidification cracking
- These materials are used in fabrication of equipment and vessels for handling and storage of sulfuric acid and phosphoric acid
Servicio de información
ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS
Ver los resultados de la prueba de limitación de responsabilidad
CONFORMANCE
| CONFORMANCES | SPECIFICATION | CLASSIFICATION |
|---|---|---|
| AWS | AWS A5.4 | E385-16 |
MECHANICAL PROPERTIES
| Classification |
Tensile Strength
MPa (ksi) |
Elongation
% |
|---|---|---|
| E385-16 Requirement | 520 (75) min. | 30 min. |
| Typical Result, As-welded | 570-590 (83-86) | 40-41 |
DEPOSIT COMPOSITION
| Classification | %C | %Cr | %Cu | %Mn | %Mo | %Ni | %P | %S | %Si |
|---|---|---|---|---|---|---|---|---|---|
| E385-16 Requirement | 0.03 max. | 19.5 - 21.5 | 1.2 - 2.0 | 1.0 - 2.5 | 4.2 - 5.2 | 24.0 - 26.0 | 0.03 max. | 0.02 max. | 0.90 max. |
| Typical Result | 0.03 | 20.2 | 1.9 | 1.3 | 4.9 | 25.2 | 0.03 | 0.00 | 0.31 |
TYPICAL OPERATING PROCEDURES
| Diameter | Polarity⁽¹⁾ |
Current
Amps |
|---|---|---|
| 3/32 in (2.4 mm) | DC+ | 40-80 |
| 3/32 in (2.4 mm) | AC | 40-80 |
| 1/8 in (3.2 mm) | DC+ | 75-110 |
| 1/8 in (3.2 mm) | AC | 75-110 |
| 5/32 in (4.0 mm) | DC+ | 95-150 |
| 5/32 in (4.0 mm) | AC | 95-150 |
| 3/16 in (4.8 mm) | DC+ | 130-200 |
| 3/16 in (4.8 mm) | AC | 130-200 |
NOTES
| Note |
|---|
| ⁽¹⁾ Preferred polarity is listed first. |