DETAILS
PIPELINER 80R is a low alloy, cellulosic stick electrode designed for high strength root pass vertical down welding of cross-country and in-plant pipe.
Features
- Same welding behavior as Fleetweld® 5P+ with a 80ksi strength
- Cross country and in-plant welding
- Deep arc penetration
- Light slag with minimal arc interference
- Q2 Lot® Control - Certificate showing actual deposit chemistry and mechanical properties per lot available online
- Excellent vertical and overhead capability
Disclaimers
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
| CONFORMANCES | SPECIFICATION | CLASSIFICATION |
|---|---|---|
| AWS | AWS A5.5 | E8010-P1 |
| CWB | AWS A5.5M | E5510-P1 |
| TUV | AWS A5.5M | E5510-P1 |
MECHANICAL PROPERTIES
| Classification |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
Charpy V-Notch
J (ft-lbs) @ -30°C (-20°F) |
Charpy V-Notch
J (ft-lbs) @ -45°C (-50°F) |
Hardness Rockwell B |
|---|---|---|---|---|---|---|
| E8010-P1 Requirement | 460 (67) min. | 550 (80) min. | 19 min. | 27 (20) min. | Info. Only | |
| Typical Result, As-welded | 480-500 (69-73) | 580-610 (84-89) | 26-28 | 34-103 (25-76) | 27-80 (20-59) | 87-93 |
DEPOSIT COMPOSITION
| Classification | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %V |
|---|---|---|---|---|---|---|---|---|---|
| E8010-P1 Requirement | 0.20 max. | 0.30 max. | 1.20 max. | 0.50 max. | 1.00 max. | 0.03 max. | 0.03 max. | 0.60 max. | 0.10 max. |
| Typical Result | 0.12-0.20 | 0.02-0.03 | 0.66-0.81 | 0.12-0.17 | 0.01-0.04 | 0.01 max. | 0.01 max. | 0.16-0.22 | 0.01 max. |
TYPICAL OPERATING PROCEDURES
| Diameter | Polarity⁽¹⁾ |
Current
Amps |
|---|---|---|
| 1/8" (3.2 mm) | DC+ | 70-130 |
| 5/32" (4.0 mm) | DC+ | 100-170 |
NOTES
| Note |
|---|
| Preferred polarity is listed first. |
| Measured with 0.2% offset |