DETAILS
Low alloy stick electrode designed for fill and cap pass welding of up to X90 grade pipe
Features
- Q2 Lot®- Control and Tested - Lot certificate available online
- Durable coating
- 80% higher productivity over traditional vertical-up pipe welding
Disclaimers
Service Information
You May Also Need
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
| CONFORMANCES | SPECIFICATION | CLASSIFICATION |
|---|---|---|
| AWS | AWS A5.5 | E10045-P2 H4R |
| CWB | CWB AWS A5.5 | E6945-P2-H4R (E10045-P2-H4R) |
MECHANICAL PROPERTIES
| Classification |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
Charpy V-Notch
J (ft-lbs) @ -30°C (-20°F) |
Charpy V-Notch
J (ft-lbs) @ -40°C (-40°F) |
Hardness Rockwell B |
|---|---|---|---|---|---|---|
| E10045-P2 H4R Requirement | 600 (87) min. | 690 (100) min. | 16 min. | 27 (20) min. | ||
| Typical Result, As-welded | 650-700 (94-102) | 710-750 (103-108) | 23-26 | 77-114 (57-84) | 42-85 (31-62) | 96-99 |
DEPOSIT COMPOSITION
| Classification | %B | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %V |
Diffusible Hydrogen
mL/100g Weld Metal |
1800F H2O - As received | 1800F H2O - After 9 hrs at 80F/80%RH |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| E10045-P2 H4R Requirement | 0.12 max. | 0.20 max. | 0.90 - 1.70 | 0.50 max. | 1.00 max. | 0.03 max. | 0.03 max. | 0.80 max. | 0.05 max. | 4 max. | 0.15 max. | 0.4 max. | |
| Typical Result | 0.004-0.0051 | 0.05-0.06 | 0.04-0.06 | 1.44-1.67 | 0.40-0.46 | 0.78-0.89 | 0.01 | 0.01 | 0.42-0.56 | 0.01 | 2-4 | 0.03-0.13 | 0.2-0.4 |
TYPICAL OPERATING PROCEDURES
| Diameter | Polarity |
Current
Amps |
|---|---|---|
| 3.2 mm (1/8 in) | DC+ | 120-170 |
| 4.0 mm (5/32 in) | DC+ | 170-250 |
| 4.5 mm (11/64 in) | DC+ | 200-300 |
NOTES
| Note |
|---|
| NOTE: This product contains micro-alloying elements. Additional information available on request. |